VehiclesEquipment

Thule, Inc.: Bike Arm Assembly Weld Defect

A detached bike arm assembly can fall into the roadway, increasing the risk of a crash.

Read the official notice →
Date
2022-10-21
Country
United States
Brand
Thule
Classification
Equipment
Units
4,759 affected
Category
Vehicles
Source
NHTSA

Copied automatically from the US National Highway Traffic Safety Administration. Details may be shortened or out of date; the official notice is the authoritative source. Disclaimer

What to do

  1. Check whether your vehicle is affected by entering its VIN (vehicle identification number) on the manufacturer's or the agency's recall lookup.
  2. Contact a dealer to book the repair. Recall repairs are normally free of charge.
  3. If the notice says not to drive or to park outside, follow that until the repair is done.

General guidance from Recall Atlas. The official notice from the US National Highway Traffic Safety Administration has the exact models, batch codes and remedy, and it takes priority.

More Thule recalls

  1. 2025-05-02
  2. DEEU
    Vehiclesinjuries

    Children's car seat (Thule) · Thule Elm

    The child seat can become separated from the base due to faulty locking. This may mean that the child seat is not properly secured, resulting in injuries in the event of an accident. The product does not comply with…

    EU Safety Gate · reported by GermanyThuleOfficial notice →
  3. 2024-04-04
  4. US
    Toys & kids

    Thule Recalls RideAlong Rear-Mounted Child Bike Seats Due to Chemical Ingestion Hazard

    The harness padding of Thule RideAlong bike seats can contain flame-retardant DecaBDE in excess of regulatory limits, posing a chemical hazard. DecaBDE can be toxic if it is ingested or comes into contact with skin or…

    CPSCAbout 8,640 (In addition, about 3,880 were sold in Canada)Official notice →
All 3 Thule recalls →

Other vehicles recalls in the United States

  1. 2022-10-21
  2. US
    VehiclesVehicle

    Daimler Vans USA, LLC: Vehicle Rollaway from Guide Bushing Fatigue

    Vehicle rollaway increases the risk of a crash.

    NHTSADaimler Vans USA, LLC124,305 affectedOfficial notice →
  3. US
    VehiclesVehicle

    Winnebago Industries, Inc.: LP Fuel Line May Contact Tire and Cause a Gas Leak

    A gas leak in the presence of an ignition source increases the risk of a fire.

    NHTSAWinnebago Industries, Inc.4,616 affectedOfficial notice →
  4. US
    VehiclesVehicle

    Altec Industries, Inc.: Jib Winch May be Operated without Outriggers Set

    Outriggers that are not set when loads are being lifted by the jib winch may cause the unit to tip, increasing the risk of injury.

    NHTSAAltec Industries, Inc.71 affectedOfficial notice →
  5. 2022-10-20
  6. US
    VehiclesVehicle

    Volvo Car USA, LLC: Loss of Drive Power

    The vehicle may lose drive power as the high voltage battery is depleted, increasing the risk of a crash.

    NHTSAVolvo Car USA, LLC15,674 affectedOfficial notice →
  7. US
    VehiclesVehicle

    Ford Motor Company: Improperly Tightened Bolt on Rear Axle

    Wheel separation from the vehicle increases the risk of a crash.

    NHTSAFord Motor Company596 affectedOfficial notice →
  8. US
    VehiclesVehicle

    Ford Motor Company: HVAC Controls May Become Inoperative

    Loss of the ability to control the defrost or defog function decreases the driver's visibility under certain driving conditions, increasing the risk of a crash.

    NHTSAFord Motor Company31,339 affectedOfficial notice →
See all vehicles recalls →